2005phyllis
04-13-2006, 09:30 PM
Today I did the stain ID kit. None of the tests showed the result it discribed. I looked back at the iron and cobalt test later and saw maybe a little improvement. The test was to pour muritic acid wait 2-3 min and then pour the iron and cobalt powder over it. The second time I did it I used a little more muritic acid. The stain got a brighter orange after sprinkling the powder in. I let it sit for about 15 min then I brushed it with a stiff hand brush. The step looks pretty good now. But when I go to use the iron and cobalt stain treatment. How am I going to scrub the whole pool. How will I ever get the sides clean as it seems like the solution has to be very concentrated. What part did the muritic acid play with the test?